Steam oxidation of TP347HFG, super 304H and HR3C – analysis of significance of steam flowrate and specimen surface finish

Volume: 50, Issue: 4, Pages: 272 - 282
Published: Jul 30, 2014
Abstract
This paper delivers an analysis of the steam oxidation of the austenitic steels used for the super heater and re-heater tubing. It compares the behaviour of TP347HFG, Super 304H and HR3C at 650 and 700°C with three different steam flowrates: 4, 16· 40 mm/s. Steam oxidation tests were performed in closed loop system for 1000 h. The differences in the steam oxidation behaviour of these materials are considered in terms of the alloy compositions...
Paper Details
Title
Steam oxidation of TP347HFG, super 304H and HR3C – analysis of significance of steam flowrate and specimen surface finish
Published Date
Jul 30, 2014
Volume
50
Issue
4
Pages
272 - 282
Citation AnalysisPro
  • Scinapse’s Top 10 Citation Journals & Affiliations graph reveals the quality and authenticity of citations received by a paper.
  • Discover whether citations have been inflated due to self-citations, or if citations include institutional bias.